Bii o ṣe le ṣe itọju itọju ooru lẹhin-forging fun awọn forgings

O jẹ dandan lati ṣe itọju ooru lẹhinayederunitori pe idi rẹ ni lati yọkuro aapọn inu lẹhin ti a ṣe. Ṣatunṣe líle ayederu, mu iṣẹ gige ṣiṣẹ; Awọn oka isokuso ti o wa ninu ilana ayederu jẹ isọdọtun ati aṣọ lati mura microstructure ti awọn ẹya fun itọju ooru.

1. Iwọn otutu otutu ti o ga: dinku líle, dinku tabi imukuro wahala ti o waye nigbati o ṣe deede itutu agbaiye, mu ṣiṣu ati lile. Dara fun irin alloy pẹlu lile lile lẹhin ti o ṣe deede.

https://www.shdhforging.com/forged-shaft.html

2. Pari annealing: imukuro isokuso ati uneven be ṣẹlẹ nipasẹ awọn forging ilana, liti awọn ọkà, imukuro awọn péye wahala ti forging, din líle, mu awọn machinability, ati ki o mura awọn ajo fun ojo iwaju ooru itoju ti awọn ẹya ara. Annealing ni kikun jẹ deede fun irin hypoeutectoid.

3. Isothermal annealing: gba diẹ aṣọ be ju pipe annealing, fe ni imukuro forging wahala, din líle. Ni pataki forgings nla, o tun le ṣee lo lati tan kaakiri hydrogen ati ki o se isejade ti funfun to muna. Ti a ṣe afiwe pẹlu ifunra pipe, o le kuru akoko annealing ati ilọsiwaju ṣiṣe iṣelọpọ.

4. Normalizing: finer pearlite le ti wa ni gba lati liti ajo; Ilọsiwajuforgingsagbara ati lile, dinku aapọn inu, mu iṣẹ gige ṣiṣẹ; Fun eutectoid irin. Mesh carbides le yọkuro.

5 spheroidization annealing: lati gba ti iyipo cementite ati ferrite be, ko nikan din líle, ati ninu awọn Ige ilana jẹ rorun lati gba dan processing dada, ninu awọn tetele quenching ni ko rorun lati gbe awọn abuku dojuijako. Spheroidizing annealing ni o dara fun ga erogba, irin ati ki o ga erogba alloy kú, irin.


Akoko ifiweranṣẹ: Oṣu kejila-02-2022